New EPR Rules 2026
Free Consultation
Recycled Polymer · Quality & Specifications

Moisture Content Testing

Moisture content testing confirms that hygroscopic recyclate is dry enough to process without hydrolytic degradation or defects.

Service lineQuality & Specifications
ForProcessors of hygroscopic recyclate such as rPET and rPC
You get3 deliverables
Part ofRecycled Polymer
What it is

Moisture Content Testing

Polymers such as PET and polycarbonate absorb moisture, which can cause chain scission and defects during melt processing. Moisture testing verifies that material is dried below the level required for reliable processing.

How we deliver

How we handle it, step by step

01Identify sensitivity

Confirm whether the polymer is hygroscopic.

02Sample

Take a representative sample after drying.

03Measure moisture

Determine moisture content by a suitable method.

04Advise drying

Recommend drying conditions to meet targets.

What's included

Your deliverables

Moisture indication
Drying-condition guidance
Process-readiness note, confirmed per enquiry
FAQ

Moisture Content Testing — questions we get

Which recyclates need drying?

Hygroscopic polymers like PET, PC and nylon require drying; polyolefins such as PE and PP are far less sensitive.

What happens if PET is wet?

Processing wet PET causes hydrolytic degradation, lowering molecular weight and part strength.